Faded loading bays on a heavily used concrete yard
This industrial yard in Great Yarmouth takes heavy truck traffic. Its loading bays had been marked in yellow thermoplastic not long before, but the lines had already faded into the concrete and were wearing away under the trucks.
We were asked to re-mark three bays, a goods in and out bay and two HGV loading bays, in something that would actually stand up to that traffic.
Before: what we found
Thermoplastic melts into tarmac, but on concrete there's no heat bond. It only grips mechanically, so without the right prep and primer it wears off and loses its colour quickly under heavy wheels. That's what had happened here.
- Yellow lines faded to the point of blending into the concrete
- Lines wearing away under the HGV traffic
The work: our approach
We swapped the thermoplastic for a hard wearing MMA system and put the time into the prep, so the new lines bond properly and last.
- Ground off the old markings with our HEPA-extracted grinding system, exposing clean concrete for the new lines to key into
- Dried the concrete fully with a gas lance
- Primed the concrete to improve the bond
- Hand applied the yellow bay lines and GOODS IN / OUT text, and white HGV 1 and HGV 2 lettering, all in MMA
The work was done out of hours.
The result
Three bright, crisp loading bays that are built to take heavy HGV traffic, backed by our 12-month workmanship warranty.
See more about our warehouse and industrial line marking and our work in Great Yarmouth, or read our guides to MMA line marking and thermoplastic line marking.
Need something similar?
Tell us about your site and we'll be in touch.
Prefer to chat to a member of the team?01603 905 022Frequently asked questions
Why did the thermoplastic fade so quickly?
On concrete, thermoplastic has no heat bond and only grips mechanically. Without proper prep and a primer it can wear and lose its colour fast under heavy traffic.
Why MMA for HGV bays?
MMA cures hard and bonds well to a properly prepared surface, so it copes with HGV traffic far better than standard paint.
Do you remove the old markings first?
Where they're failing, yes. We grind them off with dust extraction so the new lines go onto clean, sound concrete.
Can you work out of hours?
Yes. We can work evenings and weekends so your yard isn't held up.